Iron Chrome Aluminium (FeCrAl) alloys zvinhu zvisingachinjiki zvakanyanya zvinowanzo shandiswa mumaapplication ane tembiricha yekunyanya kushanda inosvika 1,400°C (2,550°F).
Aya maFerritic alloys anozivikanwa kuve ane yepamusoro yepamusoro yekurodha kugona, yakakwirira resistivity uye yakaderera density paneNickel Chrome(NiCr) dzimwe nzira dzinogona kududzira kune zvishoma zvinhu mukushandisa uye uremu hwekuchengetedza. Iyo yepamusoro yepamusoro tembiricha yekushandisa inogona zvakare kutungamira kune hurefu hwehupenyu hwezvinhu. Iron Chrome Aluminium alloys inogadzira grey Aluminium Oxide (Al2O3) yakareruka patembiricha iri pamusoro pe1,000°C (1,832°F) iyo inowedzera kusaita ngura pamwe nekuita semudziyo wemagetsi. Iyo oxide kuumbwa kunoonekwa sekuzvidzivirira uye inodzivirira kubva kupfupi kutenderera muchiitiko chesimbi kune simbi kusangana. Iron Chrome Aluminium alloys ane yakaderera mechanical simba kana ichienzaniswaNickel Chromezvinhu pamwe chete nekuderera kwesimba rinokambaira.
Giredhi | 1Cr13Al4 | TK1 | 0Cr25Al5 | 0Cr20Al6RE | 0Cr23Al5 | 0Cr19Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
Nominal composition% | Cr | 12.0-15.0 | 22.0-26.0 | 23.0-26.0 | 19.0-22.0 | 22.5-24.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
Al | 4.0-6.0 | 5.0-7.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.0 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 | |
Re | mukana | 0.04-1.0 | mukana | mukana | mukana | mukana | mukana | mukana | |
Fe | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | ||
Nb0.5 | Mo1.8-2.2 | ||||||||
Kupisa kukuru kwekushanda(°C) | 650 | 1400 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
Resisivity 20℃(Ω/mm2/m) | 1.25 | 1.48 | 1.42 | 1.40 | 1.35 | 1.23 | 1.45 | 1.53 | |
Density(g/cm³) | 7.4 | 7.1 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 | |
Thermal Conductivity pa20℃,W/(M·K) | 0.49 | 0.49 | 0.46 | 0.48 | 3.46 | 0.49 | 0.49 | 0.49 | |
Linear Kuwedzera Coefficient(×10¯6/℃)20-1000℃) | 15.4 | 16 | 16 | 14 | 15 | 13.5 | 16 | 16 | |
Yakasvika Melting Point (℃) | 1450 | 1520 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
Kusimba Kwesimba(N/mm2) | 580-680 | 680-830 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 | |
Elongation(%) | ›16 | ›10 | ›12 | ›12 | ›12 | ›12 | ›12 | ›10 | |
Section Variation Shrink Rate(%) | 65-75 | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 | |
Kasingaperi Bend Frequency(F/R) | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | |
Kuoma (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
Micrographic Structure | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | |
Magnetic Property | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | |
Hupenyu Hwekukurumidza (h/℃) | no | ≥80/1350 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 |